Home / Products / Alloy Powder / PTA
PTA
The PTA process is easily automated, ensuring consistent, repeatable weld overlays. Its concentrated heat source offers high powder efficiency and minimal iron dilution. Using powder feedstock allows for a wide range of material combinations, enabling overlays with varied hardness and performance characteristics.

Cobalt-Based Powder
Nickel-Based Powder
Ni & WC Gas Atomized Powder
Alloy | Composition | Size (µm) | HRC | Data Sheet |
---|---|---|---|---|
TMPK2105GA | TMPN+5WC | -150/+45, -180/+53 | – | – |
TMPK2110GA | TMPN+10WC | -150/+45, -180/+53 | – | – |
TMPK2115GA | TMPN+15WC | -150/+45, -180/+53 | – | – |
TMPK2120GA | TMPN+20WC | -150/+45, -180/+53 | – | – |
TMPK2125GA | TMPN+25WC | -150/+45, -180/+53 | – | – |
TMPK2130GA | TMPN+30WC | -150/+45, -180/+53 | – | – |
TMPK2135GA | TMPN+35WC | -150/+45, -180/+53 | – | – |